Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.5 MPa | 3260 psi | ASTM D882 |
ExxonMobil ESCOR™ AT 310 Cast Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |
|||
Film Tensile Strength at Break, TD | 22.5 MPa | 3260 psi | 500mm/min, Ultimate; ASTM D638 |
LG Chemical SEETEC BF500 LDPE Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem.. |