Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 165 MPa
24000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 70LS447 OPP Film
Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print su..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 342 Polyester Film
Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a vari..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 547 Polyester Film, 400 Gauge
Information provided by DuPont.
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® AG2 Polyester Film
Melinex® AG2 is a clear polyester film coated on both sides for Anti-fog and Anti-glare performanceTypical Applications: Typical applications include disposable face shields, visors, and other temp..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge
Melinex® ST328 is an exceptionally white, opaque film with a satin finish. It is pretreated on both surfaces to promote adhesion to a wide range of solvent-based and UV-curable graphics inks and va..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST329 Polyester Film, 1000 Gauge
MELINEX® ST329 has good handling properties and a unique pearlescent appearance with no pre-treatments. It is heat stabilized for applications in high temperature processes where film registration ..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Mylar® E Polyester Film, 48 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Mylar® EC Polyester Film, 500 Gauge
Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta..
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® AF Polyester Film
Melinex® AF is a clear polyester film coated both sides with an anti-fog coating. Typical Applications: Typical applications include face shields, masks, visors, and other industrial uses.Informati..