Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ISO 527-3 |
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
Chevron Phillips HiD® 9647T HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat S.. |
|||
Film Tensile Strength at Break, TD | 31.0 - 51.7 MPa | 4500 - 7500 psi | ASTM D882 |
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, TD | 31.0 - 51.7 MPa | 4500 - 7500 psi | ASTM D882 |
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, TD | 31.0 - 51.7 MPa | 4500 - 7500 psi | ASTM D882 |
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 2000 is a 2 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipmen.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended .. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
Formosa Plastics Formolene® E924ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | 2 in per min; ASTM D882 |
Chevron Phillips MarFlex® D143 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | |
Dow DOWLEX™ 2071 Linear Low Density Polyethylene DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4490 psi | ASTM D882 |
Dow DOWLEX™ 2078G Linear Low Density Polyethylene Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM-D882 |
Braskem TN2006 EVA General Film Copolymer TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. .. |
|||
Film Tensile Strength at Break, TD | 31.0 - 38.0 MPa | 4500 - 5510 psi | |
3M 6144 Economy Reinforced Water Activated Paper Tape 3M™ Economy Reinforced Water Activated Paper Tape 6144 is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and a high tack water activat.. |
|||
Film Tensile Strength at Break, TD | 31.0 MPa | 4500 psi | ASTM D882 |
M. Holland Company MAGMA® LM203-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |