Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 33100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® M33 Polyester Film, 50 Gauge, PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. the coating is heat sealable, and is an excellent moisture and..
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® M34 Polyester Film, 50 Gauge (13 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® MC2 Polyester Film, 100 Gauge (25 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A polyester film with a vacuum deposited layer of aluminum on one side and overcoated on both sides with a heat sealable PVDC copolymer. The film has exce..
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Film Tensile Strength at Break, TD 228 MPa
33100 psi
ASTM D882
DuPont Teijin Films Mylar® 50 M44E Polyester Film, One-Sided PVDC Barrier Coated, 50 Gauge  (discontinued **)&
Data provided by DuPont Packaging Polymers.A transparent, exceptionally strong polyester film, coated on one side with an oxygen and moisture barrier PVDC copolymer. It is used as a substrate in co..
Copyright © lookpolymers.com All Rights Reserved