Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Ineos Nova 3500 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill and thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma .. |
|||
Flexural Yield Strength | 68.9 - 200 MPa | 10000 - 29000 psi | Average value: 120 MPa Grade Count:19 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Flexural Yield Strength | 68.9 - 133 MPa | 10000 - 19300 psi | Average value: 103 MPa Grade Count:15 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Flexural Yield Strength | 69.0 MPa @Strain 3.50 % |
10000 psi @Strain 3.50 % |
ISO 178 |
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Spartech SP-9010 General Purpose ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Techmer ES HiFill® PP GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
PlastxWorld CEVIAN® SER91 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Westlake Plastics Dielux® PTFE filled Acetal Copolymer Dielux PTFE filled acetal copolymer is an outstanding bearing and wear material for use in both wet and dry environments. It is frequently used in place of traditional metal and plastic bearing mat.. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Formosa Plastics Formolon® APW Compound APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness.. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Formosa Plastics Formolon® AWS Compound AWS Powder Profiler Compound Series The AWS compounds have been designed for profile extrusion in indoor and non-weatherable applications and substrates for outdoor applications. They exhibit a natu.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman DURASTAR DS1010 Natural PCTA Copolyester DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to .. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman DuraStar MN610 Polymer, Natural Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very .. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Eastar AN001 Copolyester, Natural Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Eastar Copolyester BR003, Natural PCTA Copolyester EASTAR BR003 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabiliti.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Ineos Nova 3590 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable for difficult to fill and thin wall molding, Low residuals, USP Class VIApplications: Blending applications, Single service drinkware, Medical moldingExposure to g.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
PolyOne Lubri-Tech™ MP-000/15T Modified PPO - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5303 is a two-stage, mineral and floc.. |