Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 27.0 - 72.0 MPa | 3920 - 10400 psi | Average value: 48.2 MPa Grade Count:22 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |