Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 765 MPa @Temperature 23.0 °C |
111000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |