Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 152 MPa | 22000 psi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E PC 08CF is a carbon fiber-reinforced polyca.. |
|||
Flexural Yield Strength | 151.7 MPa | 22000 psi | ASTM D790 |
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
PolyOne Stat-Tech™ PI-10SS/000 Polyetherimide - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 152 MPa @Thickness 3.20 mm |
22000 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 152 MPa @Thickness 3.20 mm |
22000 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES Electrablend® PC NCF15 FR 15% Nickel-Coated Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation .. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON PFD04 PA 6 LNP* STAT-KON* PFD04 is a compound based on Nylon 6 containing 20% Glass Fiber. Added feature of this grade is: Ellectrically Conductive. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON PX93058 PA 6 (Europe-Africa-Middle East) LNP*STATKON*PX93058 is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES Plaslube® J-50/20/TF/15 Polycarbonate, 20% Glass Reinforced, PTFE Lubricated 20% Glass Reinforced, PTFE Lubricated |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill FR® PC GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
PlastxWorld CEVIAN® B5536 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Westlake Plastics Tempalux® Polyetherimide For Medical Applications Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its .. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | ASTM D790 |
Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced A 14% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polyme.. |
|||
Flexural Yield Strength | 152 MPa | 22000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible |