Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES Elastoblend® PBT GF33 IM 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES HiFill® POM CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES Luriblend® PES GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |
|||
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 172 MPa | 25000 psi | ASTM D790 |
Clariant Renol PPSSP0006 Polyphenylene Sulfide, Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 172 - 221 MPa | 25000 - 32100 psi | Average value: 192 MPa Grade Count:19 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |