Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced  (discontinued
AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr..
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric..
Flexural Yield Strength 255 MPa

@Thickness 6.40 mm
37000 psi

@Thickness 0.252 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 255 MPa

@Thickness 6.40 mm
37000 psi

@Thickness 0.252 in
2.8mm/min; ASTM D790
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 255 MPa

@Thickness 3.20 mm
37000 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 255 MPa

@Thickness 3.20 mm
37000 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface
Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 255 MPa
37000 psi
at 3.5% strain; ISO 178-A
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
Flexural Yield Strength 255 MPa
37000 psi
DIN 53455; ASTM D790
Kolon KOPA® KN132G30VO G/F Reinforced Flame Retardant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Yield Strength 255 MPa
37000 psi
DIN 53455; ASTM D790
Kolon KOPA® KN133G30 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Techmer ES HiFill FR® TPX-HTN-01031 35% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 35% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant, Heat Stabilized and High Temperature Strength UL ..
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p..
Flexural Yield Strength 255 MPa
37000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V8090 PBT+PET (Europe-Africa-Middle East)
50% Glass Fiber Reinforced PBT-PET resin
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac..
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Cheng Yu Plastic N6G20 Nylon 6, 20% Glass Filled
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Clariant Renol PA111G30IF Nylon 66, 30% Glass Fiber, Improved Flow
Data provided by Clariant Masterbatches