Polymer Property : Flexural Yield Strength = 26500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 182.7 MPa
26500 psi
ASTM D790
Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Flexural Yield Strength 183 MPa
26500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V4860HR PBT
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Flexural Yield Strength 183 MPa
26500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC
LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare.
Flexural Yield Strength 183 MPa
26500 psi
ASTM D790
Techmer ES Plastiblend® PC/PBT GF30 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Yield Strength 183 MPa
26500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Flexural Yield Strength 183 MPa
26500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Flexural Yield Strength 183 MPa
26500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
Flexural Yield Strength 183 MPa
26500 psi
ASTM D790
Toyobo T-750 Nylon, Painting Grade
Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd
Flexural Yield Strength 183 MPa
26500 psi
ASTM D790
Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced
A 25% mineral reinforced, 15% glass fiber reinforced nylon 66 offering excellent rigidity, dimensional stability and tensile strength with improved warpage control in large area parts.Data provided ..
Flexural Yield Strength 183 MPa
26500 psi
ASTM D790
Chem Polymer Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced
A glass fiber reinforced, flame retardant nylon 6,6 exhibiting excellent tensile strength and high temperature performance. The material has VO flammability rating according to UL94 testing procedu..
Flexural Yield Strength 183 MPa
26500 psi
ASTM D790
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced
A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer.
Flexural Yield Strength 183 MPa
26500 psi
Phenolic 40%, Carbon fabric 60%
Phenolic - Monsanto "SC 1008". Carbon fabric - "CCA-1"