Polymer Property : Flexural Yield Strength = 303 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 72.4 - 303 MPa
10500 - 44000 psi
Average value: 193 MPa Grade Count:120
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Flexural Yield Strength 50.0 - 303 MPa
7250 - 44000 psi
Average value: 115 MPa Grade Count:108
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Flexural Yield Strength 125 - 303 MPa
18100 - 44000 psi
Average value: 219 MPa Grade Count:28
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Flexural Yield Strength 276 - 303 MPa
40000 - 44000 psi
Average value: 290 MPa Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% ..