Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 450 MPa | 65300 psi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2 Information provided by HexCel |
|||
Flexural Yield Strength | 450 MPa | 65300 psi | ASTM D790 |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |