Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWE280 ASA Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | ISO 178 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | ASTM D790 |
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat.. |
|||
Flexural Yield Strength | 74.0 - 105 MPa | 10700 - 15200 psi | Average value: 85.4 MPa Grade Count:10 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A ACETAL HOMOPOLYMER (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing PTFE. Added features include: Internally Lubricated |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Health care grade, PTFE and silicone lubricated |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NWP100 PPE+HIPS (Asia Pacific) PPO/HIPS Unfilled high impact extrusion grade |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MFK42AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFK42AS is a compound based on PP resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 74.0 MPa @Strain 3.50 % |
10700 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flexural Yield Strength | 74.0 MPa @Strain 3.50 % |
10700 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Flexural Yield Strength | 74.0 MPa @Strain 3.50 % |
10700 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Flexural Yield Strength | 74.0 MPa @Strain 3.50 % |
10700 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 74.0 MPa @Strain 3.50 % |
10700 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Flexural Yield Strength | 74.0 MPa | 10700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |