Mechanical Properties Metric English Comments
Flexural Yield Strength 66.2 - 297 MPa
9600 - 43100 psi
Average value: 234 MPa Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Flexural Yield Strength 66.2 - 278 MPa
9600 - 40300 psi
Average value: 209 MPa Grade Count:57
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Spartech SP-9020 Premium ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE
Plaslube polytetrafluoroethylene (PTFE) lubricated acetal copolymer grades offer additional wear and friction performance over neat acetal. Typical applications include bearings, slides and small g..
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Clariant PA131 Nylon 66, Highly Impact Modified
Data provided by Clariant Masterbatches
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened
Data provided by Clariant Masterbatches
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 66.2 MPa

@Thickness 6.40 mm
9600 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron HR-60 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Flexural Yield Strength 66.2 MPa

@Thickness 6.40 mm
9600 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron HR60N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Flexural Yield Strength 66.2 MPa

@Thickness 6.40 mm
9600 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Flexural Yield Strength 66.2 MPa

@Thickness 6.40 mm
9600 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron HR-60 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Flexural Yield Strength 66.2 MPa

@Thickness 6.40 mm
9600 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Flexural Yield Strength 66.2 MPa

@Thickness 6.40 mm
9600 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron HR60N ABS Heat Resistant
High ImpactInformation provided by Bhansali