Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® EFX830ME PC Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering metallic / sparkle look with minimal flow line visibilityThis data was supplied by SABIC-.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 101R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 104R PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® 105 PC General purpose low flow Polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EX1332T PC Lexan* EX1332T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and is UV stabilized. It is availab.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LS3 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East) Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7664 PC Copolymer (Asia Pacific) Lexan* ML7664 polycarbonate (PC) siloxane resin, is a product targeting (profile) extrusion applications requiring extreme low temperature ductility. Lexan* ML7664 resin is a non-FR product availabl.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Flexural Yield Strength | 97.0 - 155 MPa | 14100 - 22500 psi | Average value: 142 MPa Grade Count:7 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML4588 PC Extrusion and extrusion blowmolding grade for aircraft applications. Meets FAR 25.853 (60 seconds/30 mils).This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Ineos Nova 1600 High Heat Crystal Polystyrene High heat resistance, Moderate flow, Good balance of strength and set-upApplications: Foam extrusion, Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant e.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Flexural Yield Strength | 97.0 MPa | 14100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |