Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 390 MPa | 56600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |