Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, TD = 228 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
LyondellBasell Petrothene® NA951000 Low Density Polyethylene
ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade
Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Westlake EP310 Low Density Polyethylene
WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Westlake Hifor Xtreme SC74842 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74842 polymer is a high strength and good clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. Films produced wit..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin
Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Copyright © lookpolymers.com All Rights Reserved