Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 450 MPa | 65300 psi | ISO 527-3 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
1% Secant Modulus, TD | 450 MPa | 65300 psi | ISO 527-3 |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |