Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.351 - 0.526 kN/m | 2.00 - 3.00 pli | |
ITW Devcon One minuteâ„¢ Epoxy Gel, Amber Information provided by ITW Devcon |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | to Steel; ASTM D3330 |
3M 2393 Premium High Temperature Masking Tape 3M™ Masking Tape 2393 is a smooth, heavy duty, mini-crepe, premium high temperature masking tape. It is specifically designed for those applications where easy removal after bake is important. This.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Photopolymer, Adhesion; ASTM D3330 |
3M 413DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | >= 0.351 kN/m | >= 2.00 pli | Government Bond |
Arlon 912-10R12-P1 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularRoll Length: 12 Yards Width, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Adhesion to ABS |
3M Controltac™ 160 Graphic Film 4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha.. |
|||
Peel Strength | 0.351 - 0.403 kN/m | 2.00 - 2.30 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive 4-mil white, opaque, polyolefin film; Chloride-free film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast and easy application; Remova.. |
|||
Peel Strength | >= 0.351 kN/m | >= 2.00 pli | Government Bond |
Arlon LW5015Rxx-P1 0.050" (1.27 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM019602 MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M PS470 White Yupo™ EDP Label Product 3M™ White Yupo™ EDP Label Products PS470 and PS472 are matte white opaque polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesiv.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Adhesion to Steel; ASTM D3330 |
3M 5481 PTFE Skived Film Tape 3M™ PTFE Skived Film Tape 5481 is a film backing with a silicone adhesive.Information provided by 3M |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Polycarbonate, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7604FP Primalyn™ White Vinyl Label Material 3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7841 Laser Toner Printable Label Material 3M™ Label Material 7841 with 3M™ Adhesive 310 is designed for continuous laser printing offering good print contrast when bar coding and excellent toner anchorage. The Adhesive 310 resists oozing .. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV022902 Soft White Vinyl Label Product 3M™ Soft White Vinyl Label Product FV22902 is a flexible vinyl label stock that offers excellent durability and some moisture resistance. This vinyl label utilizes 3M™ Adhesive F2201 which is a fr.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Polypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9828 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Peel Strength | <= 0.351 kN/m | <= 2.00 pli | 90° T-Peel, Alum/Alum; ASTM D1876-61T |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |