Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.75 kN/m | 10.0 pli | 1 oz. Cu, after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | 1 in. x 8in. Stainless steel screen at 180° pull angle |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | |
Master Bond EP21TDCS Two Component Silver Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCS is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel, Al/Al |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel, Al to Al |
Master Bond Supreme 46HT-2 Toughened, High Shear and Peel Strength Adhesive Description: Master Bond Supreme 46HT-2 is a two component epoxy adhesive featuring an attractive balance of good shear and peel strengths for high performance structural bonding and coating suitabl.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Bond Strength; ASTM D624 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | Bond Strength |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | |
Arlon IsoClad 933 Non-Woven Fiberglass Reinforced PTFE Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED). |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Bond Strength; ASTM D624 |
Arlon R35640T003 0.003" (0.0762 mm) Uncured Silicone Rubber with Polyethylene Naphthalate Substrate Design/Construction:Liner: Polyester Side 1: Uncured Silicone RubberSubstrate: Polyethylene NaphthalateAppearance: Gray gum on glass fiber fabricThis data represents typical values for the productio.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to Steel; ASTM D1000 |
3M Scotch™ 2234 Cable Jacket Repair Tape 3M™ Scotch™ Cable Jacket Repair Tape 2234 provides a cost effective and efficient means of covering and protecting damaged sections of cable jacket, thereby extending the life of the cable and red.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | T-Peel |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Faceside, to Stainless Steel, 180° Peel, 2 mil Al |
3M XP2112 Hi-Performance Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | (S1 to S1), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to PVC |
3M EPS-200 Tubing 3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to PVC |
3M EPS-300 Heat Shrink Tubing 3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to PVC |
3M EPS-400 Heat Shrink Tubing 3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Peel Strength | 1.75 kN/m @Temperature 22.0 - 24.0 °C |
10.0 pli @Temperature 71.6 - 75.2 °F |
Etched Aluminum T-Peel |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | ABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Stainless Steel 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9629FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | ABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Steel T-Peel; ASTM D1876 |
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel, Al to Al |
Master Bond Supreme 3ANHT Epoxy Adhesives for Bonding Stainless Steel Description: Master Bond Polymer System Supreme 3ANHT is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with good thermal conductivity and conve.. |