Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 10.5 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 10.5 - 11.4 kN/m
60.0 - 65.0 pli
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black
Information provided by ITW Devcon
Peel Strength 10.5 kN/m
60.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant
RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released..
Peel Strength 10.5 kN/m
60.0 pli
Cured 7 days at 25°C and 50% relative humidity
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray
RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15..
Peel Strength 10.5 kN/m
60.0 pli
Cured 7 days at 25°C and 50% relative humidity
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15..
Peel Strength 10.5 kN/m
60.0 pli
T-Peel, Etched Aluminum, 17-20 mil bondline
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Peel Strength 10.5 kN/m

@Temperature 23.0 °C
60.0 pli

@Temperature 73.4 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Peel Strength 10.5 kN/m
60.0 pli
Bell Peel Adhesion, Aluminum-etched, Cohesive Failure; ASTM D3167
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Peel Strength 10.5 kN/m
60.0 pli
180°, Polycarbonate
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 10.5 kN/m
60.0 pli
180°, Glass
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Peel Strength 10.5 kN/m
60.0 pli
Aluminum Etched, T-Peel, 17-20 mil bondline
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved