Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-120H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-620 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626SH TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-690 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-690H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |