Polymer Property : Peel Strength = 5.40 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 5.40 kN/m
30.8 pli
T-Peel, Cure Cycle, 6 hrs @ 220°F, FPL Acid Etched 6061-T6, Std Dev 1.9; ASTM D1876
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe..