Polymer Property : Tensile Strength, Ultimate = 120000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 827 MPa

@Temperature 21.1 °C
120000 psi

@Temperature 70.0 °F
Dry; ASTM D3039
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Tensile Strength, Ultimate 829 MPa

@Thickness 3.20 mm,
Temperature 760 °C
120000 psi

@Thickness 0.126 in,
Temperature 1400 °F
As Welded, Solution Annealed, and Aged; Base/Base Fracture
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Ultimate 830 MPa

@Temperature 650 °C
120000 psi

@Temperature 1200 °F
Precipitation Hardened prior to test
Special Metals NIMONIC® Alloy 81
A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content o..
Tensile Strength, Ultimate 825 MPa

@Temperature 23.0 °C
120000 psi

@Temperature 73.4 °F
Special Metals NIMONIC® Alloy 86
A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°..
Tensile Strength, Ultimate 827 MPa

@Thickness <=44.5 mm
120000 psi

@Thickness <=1.75 in
Crucible Steel Aquamet® 18 Stainless Steel
AQUAMET 18 is an austenitic stainless steel with corrosion resistance comparable to that of Type 304. Its good strength and toughness make it an ideal shafting material for workboats. It provides a ..
Tensile Strength, Ultimate 827 MPa

@Temperature 21.1 °C
120000 psi

@Temperature 70.0 °F
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..
Tensile Strength, Ultimate 825 MPa

@Temperature 23.0 °C
120000 psi

@Temperature 73.4 °F
Special Metals INCONEL® Alloy HX
A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high..