Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 800 MPa @Thickness 19.0 mm, Temperature 260 °C |
116000 psi @Thickness 0.750 in, Temperature 500 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Ultimate | 800 MPa @Thickness 6.35 mm, Temperature 20.0 °C |
116000 psi @Thickness 0.250 in, Temperature 68.0 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 800 - 950 MPa @Diameter 101 - 210 mm |
116000 - 138000 psi @Diameter 3.98 - 8.27 in |
Rm., un-machined |
Assab Steels 709M Machinery Steel ASSAB 709M is an alloyed machinery steel with high strength in small and medium sizes. As standard ASSAB 705M is supplied tough hardened requiring no further heat treatment. It can be oil hardened t.. |