Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 858.4 MPa @Temperature 210 °C |
124500 psi @Temperature 410 °F |
Wet, 0° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |