Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 917 MPa @Thickness 12.7 mm, Temperature 20.0 °C |
133000 psi @Thickness 0.500 in, Temperature 68.0 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |