Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 126.2 GPa @Temperature 24.0 °C |
18300 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel |
|||
Tensile Modulus | 126.2 GPa @Temperature 93.0 °C |
18300 ksi @Temperature 199 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G190 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |
|||
Tensile Modulus | 126.2 GPa @Temperature -54.0 °C |
18300 ksi @Temperature -65.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |