Mechanical Properties Metric English Comments
Tensile Modulus 5.10 GPa

@Temperature 23.0 °C
740 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
Tensile Modulus 5.10 GPa

@Temperature 23.0 °C
740 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Tensile Modulus 5.10 GPa

@Temperature 120 °C
740 ksi

@Temperature 248 °F
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 5.10 GPa

@Temperature 90.0 °C
740 ksi

@Temperature 194 °F
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 5.10 GPa

@Temperature 90.0 °C
740 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin..
Tensile Modulus 5.10 GPa

@Temperature 90.0 °C
740 ksi

@Temperature 194 °F
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 5.10 GPa

@Temperature 150 °C
740 ksi

@Temperature 302 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 5.10 GPa

@Temperature 90.0 °C
740 ksi

@Temperature 194 °F
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 5.10 GPa

@Temperature 23.0 °C
740 ksi

@Temperature 73.4 °F
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 5.10 GPa

@Temperature 23.0 °C
740 ksi

@Temperature 73.4 °F
90°
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber
Information provided by HexCel
Tensile Modulus 5.10 GPa

@Temperature 23.0 °C
740 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
Copyright © lookpolymers.com All Rights Reserved