Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 62.1 GPa @Temperature 82.2 °C |
9000 ksi @Temperature 180 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 62.1 GPa @Temperature 21.1 °C |
9000 ksi @Temperature 70.0 °F |
Wet, 90° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Tensile Modulus | 62.1 GPa @Temperature 177 °C |
9000 ksi @Temperature 350 °F |
Wet, 90° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Tensile Modulus | 62.1 GPa @Temperature 210 °C |
9000 ksi @Temperature 410 °F |
Wet, 90° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Tensile Modulus | 62.1 GPa @Temperature 177 °C |
9000 ksi @Temperature 350 °F |
Wet, 0° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |