Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 66.2 GPa @Temperature 23.9 °C |
9600 ksi @Temperature 75.0 °F |
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Tensile Modulus | 66.2 GPa @Temperature 19.4 °C |
9600 ksi @Temperature 67.0 °F |
CTD, 0° Direction; SACMA SRM 4R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Tensile Modulus | 66.2 GPa @Temperature 195 °C |
9600 ksi @Temperature 383 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Modulus | 66.2 GPa @Temperature -67.0 °C |
9600 ksi @Temperature -88.6 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |