Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 70.3 GPa @Temperature -67.0 °C |
10200 ksi @Temperature -88.6 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |