Polymer Property : Tensile Modulus = 856 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.90 GPa

@Temperature 90.0 °C
856 ksi

@Temperature 194 °F
ISO 527
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Tensile Modulus 5.90 GPa

@Temperature 150 °C
856 ksi

@Temperature 302 °F
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 5.90 GPa

@Temperature 23.0 °C
856 ksi

@Temperature 73.4 °F
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 5.90 GPa

@Temperature 60.0 °C
856 ksi

@Temperature 140 °F
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced
Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation ..