Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 65.5 GPa @Temperature 121 °C |
9500 ksi @Temperature 250 °F |
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Tensile Modulus | 65.5 GPa @Temperature 121 °C |
9500 ksi @Temperature 250 °F |
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Tensile Modulus | 65.5 GPa @Temperature -53.9 °C |
9500 ksi @Temperature -65.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 65.5 GPa @Temperature -67.0 °C |
9500 ksi @Temperature -88.6 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Modulus | 65.5 GPa @Temperature 77.0 °C |
9500 ksi @Temperature 171 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Modulus | 65.5 GPa @Temperature 77.0 °C |
9500 ksi @Temperature 171 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |