Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 105 - 115 MPa @Temperature 1300 °C |
15200 - 16700 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |
|||
Compressive Strength | 105 - 115 MPa @Temperature 100 °C |
15200 - 16700 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |