Polymer Property : Compressive Strength = 345 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 345 MPa

@Temperature 23.9 °C
50000 psi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Compressive Strength 345 MPa

@Temperature 177 °C
50000 psi

@Temperature 350 °F
Dry, Autoclave with Post-Cure; ASTM D695
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Compressive Strength 345 MPa

@Temperature 138 °C
50000 psi

@Temperature 280 °F
Dry, Autoclave; ASTM D695
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Compressive Strength 345 MPa

@Temperature 232 °C
50000 psi

@Temperature 450 °F
Wet; ASTM D6641
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Compressive Strength 345 MPa

@Temperature 149 °C
50000 psi

@Temperature 300 °F
Dry; ASTM D695
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..