Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 303 MPa @Temperature 177 °C |
44000 psi @Temperature 350 °F |
Open Hole, Dry; ASTM D7028 |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |