Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 315 MPa @Temperature >=210 °C |
45700 psi @Temperature >=410 °F |
Wet, 90° Direction, Ultimate |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Compressive Strength | 315 MPa @Thickness 1.60 mm |
45700 psi @Thickness 0.0630 in |
LT Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |