Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 34.3 MPa @Temperature 1100 °C |
4980 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C |
4980 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST NORMAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | >= 34.3 MPa @Temperature 1100 °C, Time 10800 sec |
>= 4980 psi @Temperature 2010 °F, Time 3.00 hour |
Cold Crushing, Specification, After firing @ 1100°C |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 34.3 MPa @Temperature 800 °C |
4980 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-45 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 34.3 MPa @Temperature 800 °C |
4980 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-Fused Silica Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 34.3 MPa @Time 86400 sec |
4980 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C |
4980 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 001 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C |
4980 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 006 Smart Cast Application Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C |
4980 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 008 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 34.3 MPa @Temperature 1000 °C, Time 10800 sec |
4980 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-120 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 1500 °C, Time 10800 sec |
4980 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CTL-Z1 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 - 39.2 MPa @Temperature 1350 °C, Time 10800 sec |
4980 - 5690 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 - 39.2 MPa @Temperature 110 °C, Time 86400 sec |
4980 - 5690 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 - 44.1 MPa @Temperature 1350 °C, Time 10800 sec |
4980 - 6400 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories IJM-1 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories joint-1 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories LPCT-18PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories SCX-85 I Special SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175S Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 34.3 MPa @Temperature 110 °C, Time 86400 sec |
4980 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |