Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 58.8 MPa @Temperature 110 °C |
8530 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 58.8 MPa @Temperature 1500 °C |
8530 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 58.8 MPa @Temperature 1400 °C |
8530 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-60 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 58.8 MPa @Temperature 1400 °C |
8530 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-70 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 58.8 MPa @Temperature 110 °C |
8530 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics THERMO PATCH Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 58.8 MPa @Temperature 1100 °C |
8530 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | >= 58.8 MPa @Temperature 1100 °C |
>= 8530 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics VELCRETE G403 Gunning Castables Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling .. |
|||
Compressive Strength | 58.8 MPa @Time 86400 sec |
8530 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 010 Smart Cast Application Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 58.8 MPa @Temperature 800 °C |
8530 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-90 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 58.8 MPa @Temperature 110 °C, Time 86400 sec |
8530 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories BPCT-170 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 MPa @Temperature 110 °C, Time 86400 sec |
8530 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 - 68.6 MPa @Temperature 1350 °C, Time 10800 sec |
8530 - 9960 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 MPa @Temperature 1350 °C, Time 10800 sec |
8530 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 - 68.6 MPa @Temperature 1500 °C, Time 10800 sec |
8530 - 9960 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTF-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 MPa @Temperature 1350 °C, Time 10800 sec |
8530 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TCH-165Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 MPa @Temperature 1500 °C, Time 10800 sec |
8530 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175S Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 58.8 MPa @Temperature 1500 °C, Time 10800 sec |
8530 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |