Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 483 MPa @Temperature 21.1 °C |
70000 psi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 483 MPa @Temperature 232 °C |
70000 psi @Temperature 450 °F |
Dry; ASTM D6641 |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |