Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 58.8 MPa

@Temperature 110 °C
8530 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST HA High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 58.8 MPa

@Temperature 1500 °C
8530 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 58.8 MPa

@Temperature 1400 °C
8530 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-60 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 58.8 MPa

@Temperature 1400 °C
8530 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-70 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 58.8 MPa

@Temperature 110 °C
8530 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics THERMO PATCH Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Compressive Strength 58.8 MPa

@Temperature 1100 °C
8530 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength >= 58.8 MPa

@Temperature 1100 °C
>= 8530 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics VELCRETE G403 Gunning Castables
Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling ..
Compressive Strength 58.8 MPa

@Time 86400 sec
8530 psi

@Time 24.0 hour
Cold Crushing
Sharadaa Ceramics ZAP 010 Smart Cast Application
Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 58.8 MPa

@Temperature 800 °C
8530 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-90 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 58.8 MPa

@Temperature 110 °C,
Time 86400 sec
8530 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories BPCT-170 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 MPa

@Temperature 110 °C,
Time 86400 sec
8530 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 - 68.6 MPa

@Temperature 1350 °C,
Time 10800 sec
8530 - 9960 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HAPT-80S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 MPa

@Temperature 1350 °C,
Time 10800 sec
8530 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MMCT-75 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 - 68.6 MPa

@Temperature 1500 °C,
Time 10800 sec
8530 - 9960 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTF-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 MPa

@Temperature 1350 °C,
Time 10800 sec
8530 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories TCH-165Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 MPa

@Temperature 1500 °C,
Time 10800 sec
8530 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories TCH-175S Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 58.8 MPa

@Temperature 1500 °C,
Time 10800 sec
8530 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories TCH-175Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved