Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 23.4 GPa @Temperature 163 °C |
3390 ksi @Temperature 325 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 149 °C |
3390 ksi @Temperature 300 °F |
0°, Wet (Immersed in water at 71°C for 7 days) |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 163 °C |
3390 ksi @Temperature 325 °F |
0°, Wet (Immersed in water at 71°C for 7 days) |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 23.0 °C |
3390 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 71.0 °C |
3390 ksi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 24.0 °C |
3390 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 71.0 °C |
3390 ksi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric Information provided by HexCel |
|||
Compressive Modulus | 23.4 GPa @Temperature 23.0 °C |
3390 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |