Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 44.8 GPa @Temperature 23.9 °C |
6500 ksi @Temperature 75.0 °F |
Open-Hole, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D6484 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Compressive Modulus | 44.8 GPa @Temperature 71.0 °C |
6500 ksi @Temperature 160 °F |
Wet |
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel |