Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 57.9 GPa @Temperature 21.1 °C |
8400 ksi @Temperature 70.0 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 57.9 GPa @Temperature 177 °C |
8400 ksi @Temperature 350 °F |
Dry, 0° Direction; ASTM D6641 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Compressive Modulus | 57.9 GPa @Temperature 21.1 °C |
8400 ksi @Temperature 70.0 °F |
Dry, 0° Direction; ASTM D6641 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Compressive Modulus | 57.9 GPa @Temperature 23.0 °C |
8400 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form Fiber: T300-3KInformation provided by HexCel |
|||
Compressive Modulus | 57.9 GPa @Temperature -59.0 °C |
8400 ksi @Temperature -74.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F593; Fiber: Toray T-300/3kInformation provided by HexCel |