Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Modulus = 60.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 60.0 GPa

@Temperature 23.9 °C
8700 ksi

@Temperature 75.0 °F
Dry, 365° Oven Cured; SACMA 1R-94
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Compressive Modulus 60.0 GPa

@Temperature 121 °C
8700 ksi

@Temperature 250 °F
Wet; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Compressive Modulus 60.0 GPa

@Temperature 288 °C
8700 ksi

@Temperature 550 °F
Dry; ASTM D6641
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Compressive Modulus 60.0 GPa

@Temperature -55.0 °C
8700 ksi

@Temperature -67.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Compressive Modulus 60.0 GPa

@Temperature 25.0 °C
8700 ksi

@Temperature 77.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Copyright © lookpolymers.com All Rights Reserved