Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 66.9 GPa @Temperature 93.3 °C |
9700 ksi @Temperature 200 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |