Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 50.3 GPa @Temperature -59.0 °C |
7300 ksi @Temperature -74.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel |