Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 60.0 GPa @Temperature 23.9 °C |
8700 ksi @Temperature 75.0 °F |
Dry, 365° Oven Cured; SACMA 1R-94 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Compressive Modulus | 60.0 GPa @Temperature 121 °C |
8700 ksi @Temperature 250 °F |
Wet; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Compressive Modulus | 60.0 GPa @Temperature 288 °C |
8700 ksi @Temperature 550 °F |
Dry; ASTM D6641 |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |
|||
Compressive Modulus | 60.0 GPa @Temperature -55.0 °C |
8700 ksi @Temperature -67.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Compressive Modulus | 60.0 GPa @Temperature 25.0 °C |
8700 ksi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |